Co: Spinel For 1535nm Passive Q-Switch;
Size: 10*10*2.046mm, T0=95%/ T0=90%,
Coating: 10*10 surface coating: S1: [email protected] 1535±5nm, S2: [email protected] 535±5nm, R=92%,
Co Spinel Crystal
Methods and Processes of Co doped Spinel Crystal Growth
Co Spinel Crystal Blank In the production of Co-doped spinel crystals, the most commonly used method is the Czochralski technique. The Czochralski method starts with heating and melting the feed material in a platinum or Iridium crucible. At an appropriate temperature, the seed crystal is dipped from top into the liquid surface of the melt, […]