Specifications Product Size/mm Quantity /pcs ①0.55%Er,Yb:glass 1.5*3*23mm 2 ②0.15%Er,Yb:glass 1.5*3*23mm 2 ③0.55%Er,Yb:glass 1.5x3x10mm 2 ④0.15%Er,Yb:glass 1.5x3x10mm 2 Structure Drawing Coating Requirements A,B: [email protected] R<0.5% C,D: [email protected] R<0.5% E,F: RE [email protected]>95% LIDT (for coating surfaces and material):0.8×10*5 J/m2 (puls duration 10-40 nsec) Coating Test Curve Er,Yb:Glass [email protected] Er,Yb:Glass [email protected] Er,Yb:Glass [email protected] Product Image
Er Yb Glass
Er,Yb:Glass For 1535nm Laser
Er,Yb:Glass For 1535nm Laser,
S1:[email protected],R<1%; [email protected]±5nm,R>99.9%; AOI: 0±1°;
S2:[email protected]±5nm, R<0.2%; [email protected], R<1% ; AOI: 0±1°;
Damage threshold :>35J/[email protected], 10ns;
Er,Yb:Glass For 1535nm Laser
Er,Yb:Glass For 1535nm Laser ;S1, [email protected] 915-960nm,& [email protected]±3nm ;S2, [email protected] 1535nm±3nm; Damage threshold >35J/[email protected], 7ns;
Er Glass (Er,Yb:Glass) Crylink have Supplied
Er Glass (Er,Yb:phosphate glass) with various Er (0.5%, 0.52%, 0.55%, 0.62%, 0.9%, 1%, 1.2%, 1.3%, 1.5%),Yb concentrations. Showing the specification about Er Glass size, concentration, coating that crylink have supplied.