3%Yb:YAG, 5%Yb:YAG, Size: 3*1*12mm, 3*1*15mm, 3*1*10mm; Coating: AR/AR @1030nm±20nm, R<0.2%; AR/AR @940nm±10nm. R<0.5%; For 1030nm laser.
Yb:YAG
The Growth and Testing of Yb:YAG Crystals (7.5%,3 inch)
Yb:YAG crystal has a melting point of 1970℃, which is a uniformly molten compound. It is usually grown by induction heating melt pulling method: First, the crystal raw material to be grown should be heated in a high temperature-resistant crucible until melted, and then adjust the temperature so that undercooling the upper part of the […]